I-GB/T EZNiCu-1 (Z508) I-Cast Iron Welding Electrode Nickel-Copper Alloy (Monel) Core kanye ne-Graphitized Coating

Incazelo emfushane:

I-GB/T EZNiCu-1 (Z508) iyi-electrode yokushisela yensimbi ephonswe ngensimbi ene-nickel-copper alloy (Monel) core kanye ne-graphitized coating.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ukushisela Insimbi Ephonswe NgensimbiI-electrode

I-Z508                                                     

I-GB/T EZNiCu-1

Incazelo: I-Z508 iyi-electrode yokushisela yensimbi ephonswe ngensimbi enomnyombo we-nickel-copper alloy (Monel) kanye ne-graphitized coating. I-AC ne-DC enezinjongo ezimbili, i-arc ezinzile, kulula ukuyisebenzisa. Ukukhiqizwa kwayo kanye nokusebenza kwayo kokusika kuseduze ne-Z308, kodwa ngenxa yokuncipha okukhulu kwensimbi efakiwe, ukumelana nokuqhekeka kuphansi. Amandla amalunga ashiselwe aphansi, ngakho-ke ayifaneleki ukushisela izingxenye ezicindezelwe.

Ukusetshenziswa: Isetshenziselwa ukulungisa ukushisela ama-grey iron castings angadingi amandla aphezulu.

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Si

Mn

Fe

S

Ni

Cu

Abanye

0.35 ~ 0.55

≤0.75

≤2.3

3.0 ~ 6.0

≤0.025

60 ~ 70

25 ~ 35

≤1.0

 

I-current enconyiwe:

Ububanzi benduku

(mm)

3.2

4.0

5.0

Ukushisela okwamanje

(A)

90 ~ 110

120 ~ 150

160 ~ 190

 

Isaziso:

1. I-electrode kumele ibhakwe ihora eli-1 cishe ngo-150℃ ngaphambi kokusebenza kokushisela;

2. Lapho ushisela, kunconywa ukusebenzisa indlela encane, futhi ubude beshidi ngalinye akufanele lidlule u-50mm. Shaya ishidi ngokushesha ngesando esincane ukuze unciphise ukucindezeleka endaweni yokulungisa ishidi futhi uvimbele imifantu ngemva kokushisela.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanyeokusebenzisekayo kokushiselaiminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 